Products
-
Poor Adhesion 2016-07-26
Causes:A (1). Under fired.A (2). Contaminated substrate.B. Overprint is higher melting and/or more viscous during firing operation than undercoat.C. Too much...
-
Coating too thin 2016-07-26
Causes:A. Excessive thinning of coating material.B. Screen mesh too fine.C. Insufficient pigment mixD. Too much heat for coating being used.Solutions:A. ...
-
Coating too heavy 2016-07-26
Causes:A. Coating too viscous.B. Screen mesh too coarse.C. Dull squeegee.D. Insufficient squeegee pressure.E. More pigment (and cost) than necessary.Solu...
-
Blister 2016-07-26
Causes:A. Moisture(1). Condensation caused by substrate being brought into warm room after being stored in cool area.(2). Condensation under print caused...